Ferro Vanadium 60
Purity:60%min
Density:9.0-9.5g/cm³
Melting Point:1750-1980 degree
Supply Ability: 100 Ton/Tons per Month
Ferro Vanadium 60 is a popular alloy that contains a high percentage of vanadium, typically around 60%. It is widely used in various industries due to its unique properties and versatility. If you are looking for high-quality ferro vanadium with an 60% vanadium content, you have come to the right place.
Ferro vanadium is primarily used as an additive in the production of steel and other alloys. It is renowned for its ability to improve the strength, hardness, and heat resistance of steel. By adding ferro vanadium to the steel production process, manufacturers can create high-quality, durable, and high-performance steel products. This includes applications in the automotive industry, construction, tools and machinery, aerospace, and many more.
|
|
|
||||||
|
V |
C |
P |
S |
||||
|
FeV60-A |
58.0-65.0 |
0.4 |
2 |
0.06 |
0.04 |
1.5 |
-- |
|
FeV60-B |
58.0-65.0 |
0.6 |
2.5 |
0.1 |
0.05 |
2 |
-- |


1. It Is an important alloy additive in iron and steel industry. It can improve the strength, toughness, ductility and heat resistance of steel. Since the 1960s, the application of ferrovanadium in the iron and steel industry has increased dramatically, to 1988 accounted for 85% of the consumption of ferro vanadium. The proportion of iron vanadium consumption in steel is carbon steel 20%, high strength low alloy steel 25%, alloy steel 20%, tool steel 15%. High strength low alloy steel (HSLA) containing vanadium iron is widely used in the production and construction of oil/gas pipelines, buildings, Bridges, rails, pressure vessels, carriage frames and so on due to its high strength.
2. In the non-ferrous alloy is mainly used to produce vanadium ferrotitanium alloy, such as Ti-6Al-4V, Ti-6Al-6V-2Sn and
Ti-8Al-1V-Mo. Ti-6al-4v alloy is used in the manufacture of aircraft and rockets excellent high temperature structural materials, in the United States is very important, the output of titanium vanadium ferroalloy accounted for more than half. Ferro vanadium metal can also be used in magnetic materials, cast iron, carbide, superconducting materials and nuclear reactor materials and other fields.
3. Is mainly used as an alloy additive in steelmaking. The hardness, strength, wear resistance and ductility of steel
4. Suitable for alloy steel smelting, alloy element additive and stainless steel electrode coating, etc. This standard applies to the production of niobium pentoxide concentrate as raw material for steel making or casting additives, electrode as alloy agent, magnetic materials and other uses of iron vanadium.


A: We had been in this line for more than 30 years, we can not only provide you high quality products with competitive price, but also we can supply good technique service ,which can help you solve problems.
A:Always a pre-production sample before mass production;
maq per Qat: ferro vanadium 60, China ferro vanadium 60 manufacturers, suppliers